7075 ALUMINUM PLATE
Alloy 7075 aluminum plates are the outstanding member of the 7xxx series and remains the baseline among the highest strength alloys available.
Zinc is the primary alloying element giving it strength comparable to steel. Temper T651 possesses good fatigue strength, fair machinability, resistance
welding and corrosion resistance ratings. Alloy 7075 in temper T7x51 has superior stress corrosion resistance and replaces the 2xxx alloy in the most
critical applications. It is widely used by the aircraft industry with the typical specifications of ASTM B209, AMS-QQ-A-250/4, as well as many end users
requirements.
Applications:
- Air-frame structures
- Highly stressed aircraft parts
Silicon | 0.4 |
Iron | 0.5 |
Copper | 1.2-2.0 |
Manganese | 0.3 |
Magnesium | 2.1-2.9 |
Chromium | 0.18-0.28 |
Zinc | 5.1-6.1 |
Titanium | 0.2 |
Others, each | 0.05 |
Others, total | 0.15 |
Balance, Aluminum |
Thickness | Tensile Strength | Yield Strength | Elongation |
---|---|---|---|
In. | KSI | KSI | % |
.250-4.00 | 83-73 | 73-63 | 13-11 |
Miele Metal stocks a full product line in tempers T651 and T7351 with widths 48.5" and 60.5". All are certified to ASTM B209, AMS-QQ-A-250/12